AS 2136: 12/31/1977 Method for detecting the susceptibility of copper and its alloys to stress corrosion cracking using the mercurous nitrate test

Original price was: $40.00.Current price is: $16.00.

Method for detecting the susceptibility of copper and its alloys to stress corrosion cracking using the mercurous nitrate test 12/31/1977

PDF Format Searchable Printable Bookmarks

ISBN(s): 0726213896

Specifies requirements for the testing reagent and describes two methods of preparation of the reagent. Preparation of test pieces, procedures for carrying out the test and details for the preparation of a test report are given.

Attributes

Edition 1st
Published 12/31/1977
ISBN(s) 0726213896
Number of Pages 3
File Size 1 file, 220 KB
Product Code(s) 10087647, 10087652, 10087650